TPEE Grade Selection: A 6-Step Guide by Hardness & Temperature
Time of issue:2026-11-12 09:00
source:
author:

Selecting TPEE by hardness alone is the most common buying mistake. Start with Shore D to narrow the field, cross-check flexural modulus because two grades of the same hardness bend differently, leave 20–30 °C between maximum service temperature and melting point, match MFR to your equipment, then screen for flame retardancy or chemical exposure — and always finish with a test on the real part.
Why a grade table is not a selection method
A table of twenty grades and their applications is useful, but it does not tell you which grade is right for *your* part. The reason is simple: TPEE properties trade off against one another. Push hardness up and low-temperature flexibility falls. Raise the melting point and processing becomes narrower. Add flame retardancy and you may change the hydrolysis behaviour.
A method beats a table. Here is the one our application engineers use.
Step 1 — Start with Shore D, but treat it as a filter
Hardness band | Typical character | Common applications |
25D–40D | Soft, high elasticity, good low-temperature retention | Seals, soft grips, flexible tubing, sports grips |
45D–60D | Balanced strength and elasticity; the mainstream band | CVJ boots, corrugated tube, cable jacket, hose |
63D–82D | High stiffness, high strength, better oil resistance | Gears, structural parts, rigid tubing, cable sheath |
Use this band to discard unsuitable candidates, not to pick the final grade.

Shore D is a filter, not the whole answer
Step 2 — Cross-check flexural modulus
Two grades with the same Shore D can differ substantially in flexural modulus. If your part sees bending loads, specify from the modulus column. A clip that snaps back, a beam that deflects and a boot that folds all need different modulus values at the same hardness.
Step 3 — Compare melting point with service temperature
Leave a minimum safety margin of 20–30 °C between the highest service temperature and the melting point. For an under-hood location reaching 130 °C, a melting point of at least 160 °C is the floor — and above 200 °C is preferable to avoid creep and dimensional drift. Remember that melting point is a phase change, not a continuous-use rating; the long-term thermal ceiling is a separate value on the datasheet.
Step 4 — Match MFR to the process
Higher-MFR grades suit high-speed extrusion and thin-wall injection molding. Lower-MFR grades need more back-pressure and higher temperatures. Confirm that your screw design and barrel capacity can handle the viscosity range before committing to a grade. TPEE melt viscosity is unusually temperature sensitive, so verify at the nozzle, not only at the barrel setpoint.

Match MFR to the process window
Step 5 — Screen the special requirements
Requirement | What to specify | Why a standard grade may fail |
Flame retardancy | Halogen-free V-0 grade with CTI data | Additives can bloom or attack copper |
Hot water / humidity | Hydrolysis-stabilised package | Harder grades can be *less* water resistant |
Outdoor UV | Light-stabilised or carbon-black grade | Unstabilised TPEE yellows and loses elasticity |
Oil and fuel | Grade verified against the actual fluid | Generic resistance data is not application data |
Low-temperature flex | Grade with documented brittleness temperature | Hardness does not predict cold flex |
Step 6 — Test the real part
No grade selection is complete without a trial on the actual geometry under real service conditions. Bend radius, wall thickness, weld-line position and mould temperature all change the outcome. Request samples, run them on your tool, and measure the property that actually matters — cycles to failure, not just tensile strength.
Where customisation enters the method
Steps 1–4 usually land on a standard grade. Step 5 is where requirements collide. A cable that needs halogen-free V-0 *and* 90 °C water resistance, or a boot that needs minus 40 °C flex *and* oil resistance, rarely has a perfect catalogue match.
At DOWREN's own Dowren-Daolun plant in Changzhou, we handle these collisions by compounding: the base resin is chosen for the dominant requirement, then the stabiliser, flame-retardant or toughening package is adjusted for the second. That is why our selection guide always ends with a choice — standard grade, or modified compound.
A worked example
A customer needed a 55D part for an outdoor cable application, with UV resistance, halogen-free V-0 and low-temperature bend performance. No single standard grade met all three. We supplied a modified 55D compound with a light-stable package, a halogen-free FR system and a soft-segment selection for cold flex, along with the TDS, a lot-level COA and 5 kg trial samples. The part passed their bend and flame tests without changing the tool.
Documents and next step
Every recommendation from our Changzhou plant includes a grade-specific TDS with test methods and units, a lot-level COA, RoHS and REACH declarations, and processing guidance. Send us your hardness target, service temperature, media and certification requirement — we will return a shortlist with samples in 1 kg, 5 kg or 10 kg moisture-barrier packs.
DOWREN NEW MATERIAL (HENAN) CO.,LTD
TELL:Selina.Liu +86-0393-8993626 / +86 18137458807
ADD:150 meters north of the intersection of Zhongyuan Road and Pushang Road, Puyang City,Henan Province
EMAIL:dowren@dowren.com
WhatsApp (+86 18137458807)